The Use And Maintenance Of Gel Battery

The use and maintenance of Gel Battery
 1) how to enable new Gel Battery
Before the new battery is activated, the surface of the plate will have a certain degree of oxidation. The longer the storage time, the more serious the oxidation. After adding the electrolyte, there will be a sudden warming phenomenon, charging will show a larger resistance, so that charging difficult. Therefore, the opening of the new battery should be done: add electrolyte, the static release 6h or so, until the electrolyte completely soaked plate, the temperature dropped to 35 ℃ below, and then connected to the power supply for charging; charging current strictly controlled within the specified range , Such as charging the process of heating too high, more than 45 ℃, can reduce the charging current or stop charging; 1 to 2 times charge and discharge cycle to achieve the rated capacity.
2) how the new colloidal battery to initial charge
The battery is positive and negative were connected to the power supply positive and negative, first with the initial charge current charged to the electrolyte release bubbles, single cell voltage rose to 2.3 ~ 2.4V. And then the current is reduced to 1/2 the initial charge current, continue to charge the electrolyte to release violent bubbles, electro-hydraulic specific gravity and voltage for 3h stable for the same time. The total charge time is about 45 ~ 65h. During the charging process should always measure the temperature of the electrolyte, if the temperature is too high, the current can be halved, stop charging or cooling method, the temperature control at 35 ~ 40 ℃. After the initial charge is completed, if the specific gravity of the electrolyte is not specified, the application of distilled water or specific gravity of 1.4 to adjust the electrolyte after charging 2h, until the proportion of compliance with the provisions so far. New Gel Battery after the first charge is often less than the rated capacity, should be charged, discharge cycle. With a rated capacity of 1/20 of the current discharge to a single voltage drop to 1.75V, and then add sufficient charge current. After a charge and discharge cycle, if the capacity is still lower than the rated capacity of 90%, should be carried out once charge and discharge cycle.
3) how to maintain Gel Battery
A. Gel Battery in the course of the use of water evaporation and charging water electrolysis will make the liquid level is reduced, so every summer 5 to 6 days, winter every 10 to 15 days should check the liquid level, and as needed Add distilled water. In addition to leakage due to leakage caused by the liquid, not allowed to add electrolyte, or electrolyte ratio will be higher than 1.300, so as to shorten the life of Gel Battery. Colloidal battery surface should be higher than the plate 15mm, the liquid surface is too easy to spill, corrosion around the parts, there may be positive and negative pole pile conduction, causing self-discharge; liquid level is too low, easy to reveal the upper surface of the plate, Not only will reduce the capacity of Gel Battery, and exposed plate will soon cure.
B. The use of Gel Battery due to different working conditions, often lack of charge (especially short-distance vehicles). One of the following circumstances should be added to charge: ① electrolyte weight dropped to 1.200 below; ② winter discharge more than 25%; ③ summer discharge more than 50%; ④ light dim; ⑤ start powerless. Supplemental charging is carried out in two phases. The first stage to the rated capacity of 1/10 of the current charge to a single grid voltage of 2.4V, the electrolyte began to release bubbles so far, generally 10 ~ 11h. The second stage will halve the current until sufficient, usually 3 ~ 5h. If the specific gravity of the electrolyte is not specified, it should be adjusted in the same way as the initial charge. C. Use of Gel Battery in winter should pay attention to: ① to ensure that the electrical pile and wire joints connected firmly, good contact; ② Gel Battery installed on the insulation device to avoid the temperature is too low, the resistance increases; ③ according to the provisions of the proportion of electrolyte; In the engine running, the engine to the colloidal battery charging distilled water, so that water and electrolyte mixed uneven caused by icing; ⑤ engine cold start should be preheated, each starting time does not exceed 5s, repeat the start should be separated by 15s, If the three starts unsuccessful, should be checked, do not blindly restart; ⑥ often to keep the battery in a fully charged state, to prevent the proportion of electrolyte to reduce the ice, or even damage the colloidal battery.